B-10A Plastic Chip Carrier Cracking Task Group

Cochair Christina Landon, Naval Surface Warfare Ctr
Staff Liaison
Staff Liaison
Committee Charter This task group was formed based on concerns raised at the Surface Mount Council regarding cracking observed in plastic chip components. They developed technical document IPC-SM-786 (Recommended Procedures for Handling of Moisture Sensitive Plastic IC Packages) to address this. Subsequently, they joined with JEDEC to develop replacements for IPC-SM-786 to reflect current technology. J-STD-020A.